Analysis and Preventive Measures for Scaling in Mist Eliminator of WFGD System

DANG Long1, ZHANG Xiao-ling2, WANG Zhi1, CHEN Jun1, SHI Chen-xin1   

  1. 1. Shaanxi Huadian Puchen Power Generation Co., Ltd, Pucheng 715501, China;
    2. Huadian Electric Power Research Institute, Hangzhou 310030, China
  • Received:2016-11-16 Revised:2017-01-06 Published:2017-02-28 Online:2017-02-28

Abstract: In a power plant,the scaling accident of mist eliminator occured frequently in the 660 MW unit flue gas desulfurization system. The problem had seriously affected the normal operation. To solve this problem, this paper analyzed the scaling samples and the factors which affected the operation of the mist eliminator. It is concluded that the mixed scales formed by the deposition and the crystallization reaction between the flue gas and the slurry. The mixed scales and the washing is not in time are the reasons for the failure of the mist eliminator. For this problem,a series of preventive measures are put forward

Key words: desulfurization, mist eliminator, scaling, blocking, preventive measure